The real cost to manufacture a PCB encompasses everything that goes into making the product: the materials and other value-added supplies, machine and personnel costs, and most importantly, your quality. A hard look at real costs seems wholly appropriate.
Alternate Metallization Processes
Traditional electroless copper and electroless copper immersion gold have been primary PCB plating methods for decades. But alternative plating metals and processes have been introduced over the past few years as miniaturization and advanced packaging continue to develop.
Technology Roadmaps
In this issue of PCB007 Magazine, we discuss technology roadmaps and what they mean for our businesses, providing context to the all-important question: What is my company’s technology roadmap?
- Articles
- Columns
Search Console
- Links
- Media kit
||| MENU - pcb007 Magazine
Estimated reading time: 5 minutes
The Plating Forum: An Overview of Surface Finishes
Surface finish R&D departments on the supplier side have been very busy coming up with new finishes to meet the everchanging demands of the electronics industry. Today, designers have wide variety of finishes to choose from: HASL (hot air solder leveling), electrolytic nickel gold, OSP (organic solderabilty preservative), ENIG (electroless nickel/immersion gold), I-Ag (immersion silver), I-Sn (immersion tin), ENEPIG (electroless nickel/electroless palladium/immersion gold), EPIG (electroless palladium/immersion gold), EPAG (electroless palladium/auto-catalytic gold), DIG (direct immersion gold), and ISIG (immersion silver/immersion gold). In addition, most finishes offer variations within their process; specifying thickness of the layers and the type of electrolyte is used to meet specific performance criteria.
Historically, HASL was among the first finishes that saw wide use as a solderable finish. HASL was accompanied by tin-lead reflow where it was suitable, as long as tin-lead soldering remained the primary assembly method. Both HASL and tin-lead reflow required a thermal excursion. The technology (mostly double-sided) at that time could tolerate it.
OSP was introduced as a simpler, faster, and safer procedure. OSP gained market share as long as the primary assembly method required only a single excursion to tin-lead reflow temperature.
With the introduction of SMOBC (solder mask over bare copper), the dominant finishes were HASL and OSP for pads and electrolytic nickel/electrolytic hard gold for contacting fingers.
As MLB (multilayer boards) and surface mount were introduced, HASL topography (lack of planarity) became a problem at assembly as the pad size continued to shrink. ENIG and OSP became the better choices. ENIG had the advantage over OSP in that it withstands multiple thermal excursions required at assembly. ENIG was also aluminum wire bondable and a good metallic contacting surface. All these advantages justified the higher cost and complexity of processing associate with ENIG.
For a few years, ENIG, HASL, OSP, and electrolytic nickel gold were the staple for the industry, with HASL and OSP for simpler products that require a single thermal excursion at assembly. ENIG was the choice for surface mount and BGA (ball grid array) used for surface mount, where co-planarity was paramount. Electrolytic nickel gold was used to plate hard gold over nickel for insertion fingers and with a thicker, soft gold layer it was the choice for gold wire bonding.
With the introduction of lead-free (LF) solder—an example is SAC 305—the reflow temperature was increased from 230oC to 260 oC. Standard OSPs could not withstand the reflow temperature of LF solder and a new generation of high temperature (HT) OSPs came to the market. This class of OSPs could withstand the increased reflow temp of LF solder and was capable of withstanding multiple thermal excursions.
In the same time frame, the industry saw the introduction of immersion silver and immersion tin. Immersion silver (a metallic surface finish) is a solderable, coplanar contacting surface. Although silver had some limitations like tarnishing and creep corrosion, it has its place with certain process modifications to contain tarnishing and creep corrosion. Immersion tin became a viable finish, particularly for press fit type connectors where its lubricity came in play. Of course, it was solderable for LF solder. For immersion tin, the IPC specified a thick layer (40 µin or one micron) to counter the natural tendency to form an IMC (copper-tin intermetallic) on storage or thermal excursion. If the IMC works its way to the surface it would render the surface non-solderable.
With continued miniaturization, electrolytic nickel gold for gold wire bonding became a problem as it required electrical continuity through bussing. There was a need for a gold wire-bondable surface that was non-electrolytic; this resulted in the development of the ENEPIG (electroless nickel, electroless palladium, immersion gold) surface finish. The palladium layer between the nickel and the surface gold is a diffusion barrier to the migration of nickel to the surface, which can create bond failures. ENEPIG offered all the advantages of ENIG plus gold wire bonding.
As the use of wireless networks and handheld devices continued to grow, massive data is transmitted through printed circuit boards in the form of high frequency RF signals. It became clear that the electroless nickel layer in ENIG and ENEPIG will create signal loss. This brought about the development of nickel-free surface finishes. At present there is commercially available EPIG and EPAG, both nickel-free. Another finish that fits the bill is thicker DIG. I wrote about DIG in a previous column. A new addition to this group is ISIG, which is presently under development.
On the manufacturing end, board shops choose the surface finishes they offer to their customer base. The newer finishes that are in limited demand are relegated to contract plating shops. These shops offer a wider variety of surface finishes to the board shop, which will, in turn, subcontract their services. As the demand increases, the board shop will eventually set up the capability in house.
Designers have a lot of choices where they balance availability, cost, manufacturability, and performance. In some instances, specific finishes are the only option (for example, nickel-free finishes for RF signal propagation). Designers also must specify the thickness that would meet their design criteria.
The IPC Plating Committee has put out specifications for ENIG, I-Ag, I-Sn, and ENEPIG. In the specifications, a thickness range for the different layers is included, as well as performance criteria. Designers can call out the IPC specification in lieu of specifying thickness and performance. It is important to note here that designers have the option of taking exception with any parts of the specification. Such exceptions are noted in the design drawings.
All the finishes discussed here have big pluses as well as certain limitations. All the finishes are in use today. Hardly any have been obsoleted. Simpler board designs and performance expectations are readily met by simpler finishes like HASL, I-Ag, I-Sn, and OSP. The more sophisticated designs require more complex finishes like ENIG, ENEPIG, EPIG/EPAG, DIG, and ISIG to meet the designer’s performance expectations.
This column originally appeared in the August 2021 issue of PCB007 Magazine.
More Columns from The Plating Forum
The Plating Forum: Reduction Assisted Immersion Gold for ENEPIG Surface FinishThe Plating Forum: Surface Finish Evolution from Conventional to Advanced
The Plating Forum: Plating in Electronic Applications
The Plating Forum: How the Pandemic Impacted PCB Manufacturing
The Plating Forum: The Significance of IPC ENIG Specification 4552 Revision B
The Plating Forum: The IPC Surface Finish Specifications
The Plating Forum: DIG—The Next Generation
The Plating Forum: RAIG (Reduction Assisted Immersion Gold) for Gold Surface Finishes